000 00698nam a22001577a 4500
008 150717b2014 xxu||||| |||| 00| 0 eng d
100 _aKadam,Dadasaheb Nanasaheb
245 _aTo study the relationship between microstructure and hydrogen induced cracking of carbon managanese steel with respect to heat treatment
_ba dissertation report
260 _aJaipur
_bDept.of.Metallurgical and Materials Engineering.Malaviya National Institute of Technology
_c2014.
300 _aix,68 p.
500 _a(Dissertation report of Master Degree.Under the guidance of Dr.V.K .Sharma).
650 _aMetallurgical and Materials Engineering
650 _aHeat treatment
700 _aSharma,V K
942 _cDS
999 _c63601
_d63601